This set of Material Science Multiple Choice Questions & Answers (MCQs) focuses on Material Science Set 14

Q1 | Positive screw dislocation is represented by
  • 0
Q2 | Recrystallisation temperature of Iron is………..
  • 727 °c
  • 775 °c
  • 800 °c
  • 700 °c
Q3 | Recrystallization rate varies in the following manner with temperature
  • linearly increasing
  • linearly decreasing
  • exponential
  • logarithmic
Q4 | Repeatable entity of a crystal structure is known as
  • crystal
  • lattice
  • unit cell
  • miller indices
Q5 | Requirement for cross-slip movement of dislocation
  • preferred slip plane
  • preferred slip direction
  • no preferred slip plane
  • no preferred slip direction
Q6 | Round brackets are used to represent crystallographic             
  • point location
  • direction
  • plane
  • none of the above
Q7 | Schottky defect found in                   
  • metal
  • non-metal
  • ionic
  • plastics
Q8 | Schottky defect have missing of
  • cation
  • anion
  • electron
  • both a&b
Q9 | Schottky-defect in ceramic material is
  • interstitial impurity
  • vacancy- interstitial pair of cations
  • pair of nearby cation and anion vacancies
  • substitution al impurity
Q10 | Schottky-defect is of this type.
  • point
  • line
  • volume
  • surface
Q11 | screw dislocations have burger vectorfor dislocation line
  • perpendicul ar
  • parallel
  • inclined
  • first perpendicul ar then parallel
Q12 | screw dislocations includes
  • tension lattice strain
  • compression lattice strain
  • shear lattice strain
  • all
Q13 | Sharp break in dislocation line that is in slip plane .
  • jog
  • kink
  • either jog or kink
  • none
Q14 | slip plane orientation after grain boundary
  • by pass
  • crosses
  • change
  • none of the above
Q15 | Slip systems having two types one is glide& another one is                     
  • climb
  • slip
  • twinns
  • none of the above
Q16 | Square brackets are used to represent crystallographic                     
  • point location
  • direction
  • plane
  • none of the above
Q17 | Stacking fault energies are in the range of
  • 0.01-0.1j/m2
  • 0.01-0.1j/cm2
  • 0.1-10 j/m2
  • 0.1-10 j/m2
Q18 | Stacking fault is type of defect
  • point
  • line
  • volume
  • surface
Q19 | Surface decarburisation in steels in cold working .
  • does not occurs
  • occurs
Q20 | Surface decarburisation in steels in hot working .
  • does not occurs
  • occurs
Q21 | Surface finish is good in
  • hot working
  • cold working
  • both a and b
  • can’t say
Q22 | Surface finish is poor in
  • hot working
  • cold working
  • both a and b
  • can’t say
Q23 | Temp. required for cold working is
  • above 100°c
  • below 100°c
  • below recrystalliza tion
  • above recrystalliza tion
Q24 | Temp. required for hot working is
  • above 100°c
  • below 100°c
  • below recrystalliza tion
  • above recrystalliza tion
Q25 | The arrangement of multiple unit cells together is called
  • crystal structure
  • unit cell
  • lattice constant
  • lattice angle